MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® C276 Nickel Superalloy Tubing, Annealed
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.

Data provided by the manufacturer, Special Metals.

Key Words: C-276
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 105400 psiTypical
Tensile Strength, Yield 45400 psi
@Strain 0.2 %
Typical Annealed
Elongation at Break 70 %Typical Annealed
Modulus of Elasticity 205 GPa
Poissons Ratio 0.307
Shear Modulus 79.0 GPa
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.0002at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.427 J/g-°C
Thermal Conductivity 9.80 W/m-K
Melting Point 1325 - 1370 °C
Solidus 1325 °C
Liquidus 1370 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.010 %
Chromium, Cr 14.5 - 16.5 %
Cobalt, Co <= 2.5 %
Iron, Fe 4.0 - 7.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 15 - 17 %
Nickel, Ni 59 %As remainder
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.080 %
Sulfur, S <= 0.030 %
Vanadium, V <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® C276 Nickel Superalloy Plate
Special Metals INCONEL® Alloy 686 Nickel Superalloy Plate (UNS N06686)
Special Metals INCONEL® Alloy 718
Inconel 587 Nickel Alloy
Special Metals INCONEL® Alloy 600

NINCO02 / 17435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.