MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® Nylene 4114 Nylon 66, Impact Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Impact-modified nylon 6/6 molding resin with high impact strength and increased flexibility. Recognized by Underwriters Laboratories and is approved for automotive use under Ford Motor Company specification ESA-M4D379-A and Chrysler Corporation specification MS-DB41 CPN 3466.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.014 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 49.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 1860 MPaASTM D638
Flexural Modulus 1740 MPaASTM D790
Izod Impact, Notched 180 J/m
@Temperature -40.0 °C
ASTM D256
 860 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 258 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
Flammability, UL94 HB
@Thickness 0.830 mm
Natural
 
Descriptive Properties
Automotive ApprovalsFord & Chrysler spec.: ESA-M4D379-A & MS-DB41 CPN 3466 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 41 NT Impact Modified Nylon 66
Wellman Wellamid® XT1573-N Impact Modified Nylon 66
Overview of materials for Nylon 66, Impact Grade
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
Trinseo Plexiglas® V825 Acrylic

PNYLEN954 / 221486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.