MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sodium, Na
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 g/cc0.0351 lb/in³
Vapor Pressure  1.43e-10 bar
@Temperature 100 °C
1.07e-7 torr
@Temperature 212 °F
 1.81e-7 bar
@Temperature 200 °C
0.000136 torr
@Temperature 392 °F
 0.0000185 bar
@Temperature 300 °C
0.0139 torr
@Temperature 572 °F
 0.00519 bar
@Temperature 500 °C
3.89 torr
@Temperature 932 °F
 0.140 bar
@Temperature 700 °C
105 torr
@Temperature 1290 °F
 1.20 bar
@Temperature 900 °C
900 torr
@Temperature 1650 °F
 2.00 bar
@Temperature 980 °C
1500 torr
@Temperature 1800 °F
 5.10 bar
@Temperature 1120 °C
3830 torr
@Temperature 2050 °F
 10.0 bar
@Temperature 1230 °C
7500 torr
@Temperature 2250 °F
 20.0 bar
@Temperature 1370 °C
15000 torr
@Temperature 2500 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 22.98977122.9897711995
Atomic Number 1111
Thermal Neutron Cross Section 0.54 barns/atom0.54 barns/atom
X-ray Absorption Edge 11.478 Å11.478 ÅK
Critical Temperature 2300 °C4170 °F
Electrode Potential -2.71 V-2.71 V
Electronegativity 0.930.93Pauling
Ionic Radius 0.970 Å0.970 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 0.86 g/A/h0.86 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 0.100.10
Tensile Strength, Ultimate <= 10.0 MPa<= 1450 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000433 ohm-cm
@Temperature 0.000 °C
0.00000433 ohm-cm
@Temperature 32.0 °F
 0.00000477 ohm-cm
@Temperature 20.0 °C
0.00000477 ohm-cm
@Temperature 68.0 °F
 0.00000623 ohm-cm
@Temperature 77.0 °C
0.00000623 ohm-cm
@Temperature 171 °F
 0.00000686 ohm-cm
@Temperature 98.0 °C
0.00000686 ohm-cm
@Temperature 208 °F
solid
 0.00000943 ohm-cm
@Temperature 98.0 °C
0.00000943 ohm-cm
@Temperature 208 °F
liquid
 0.00002214 ohm-cm
@Temperature 400 °C
0.00002214 ohm-cm
@Temperature 752 °F
 0.00004635 ohm-cm
@Temperature 800 °C
0.00004635 ohm-cm
@Temperature 1470 °F
 0.00007376 ohm-cm
@Temperature 1100 °C
0.00007376 ohm-cm
@Temperature 2010 °F
Magnetic Susceptibility 5.1e-75.1e-7cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 114 J/g49.0 BTU/lb
Heat of Vaporization 4208 J/g1810 BTU/lb
CTE, linear 71.0 µm/m-°C
@Temperature 20.0 - 100 °C
39.4 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 1.235 J/g-°C0.2952 BTU/lb-°F
Thermal Conductivity 135 W/m-K937 BTU-in/hr-ft²-°F
Melting Point 97.8 °C208 °F
Boiling Point 883 °C1620 °F
 
Component Elements PropertiesMetricEnglishComments
Sodium, Na 100 %100 %
 
Descriptive Properties
CAS Number7440-23-5

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Aluminum, Al
Cesium, Cs
Gold, Au
Mercury, Hg

AMENa00 / 65

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.