MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® C3U10 PA6/66 FR (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connectors etc. in household appliance.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Melt Flow 258 g/10 min
@Load 5.00 kg,
Temperature 275 °C
258 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 10 %10 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 1.10 GPa160 ksiISO 527-1/-2
Flexural Strength 40.0 MPa5800 psiat max force; ISO 178
Flexural Modulus 1.10 GPa160 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 350 V350 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °FInjection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C3U PA66/6 (Conditioned)
BASF Ultramid® C31 01 PA6/66
Akro-Plastic Akromid® C3 1 (4546) PA66/6 Conditioned
BASF Ultramid® C33 PA6/66
BASF Ultramid® C33 01 PA66/6 (Conditioned)

PBASG0302 / 131935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.