MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Victrex APTIV™ 1000 Series Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: APTIV 1000 series films are the unfilled semi-crystalline films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom. APTIV 1000 has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen free and ease of processing makes APTIV films a technology enabler for our customers and end users.

All information provided by Victrex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
@Temperature 23.0 °C
ISO 1183
Water Absorption 0.040 %
@Thickness 0.0500 mm,
Temperature 23.0 °C
Equilibrium, 50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD >= 150 %
@Thickness 0.0250 mm
ISO 527-3
 >= 150 %
@Thickness 0.125 mm
ISO 527-3
 >= 150 %
@Thickness 0.0500 mm
ISO 527-3
 >= 150 %
@Thickness 0.250 mm
ISO 527-3
 255 %
@Thickness 0.0500 mm,
Temperature 200 °C
ISO 527-3
Film Elongation at Break, TD >= 150 %
@Thickness 0.0250 mm
ISO 527-3
 >= 150 %
@Thickness 0.125 mm
ISO 527-3
 >= 150 %
@Thickness 0.0500 mm
ISO 527-3
 >= 150 %
@Thickness 0.250 mm
ISO 527-3
Tensile Modulus 2.30 GPa
@Thickness 0.250 mm
MD; ISO 527-3
 2.30 GPa
@Thickness 0.250 mm
TD; ISO 527-3
 2.30 GPa
@Thickness 0.125 mm
TD; ISO 527-3
 2.40 GPa
@Thickness 0.125 mm
MD
 2.50 GPa
@Thickness 0.0500 mm
MD; ISO 527-3
 2.50 GPa
@Thickness 0.0500 mm
TD; ISO 527-3
 2.60 GPa
@Thickness 0.0250 mm
MD; ISO 527-3
 2.80 GPa
@Thickness 0.0250 mm
TD; ISO 527-3
Tear Strength 6.00 kN/m
@Thickness 0.0500 mm
MD, Trouser; ISO 6383-1
 8.00 kN/m
@Thickness 0.0500 mm
TD, Trouser; ISO 6383-1
Film Tensile Strength at Break, MD 110 MPa
@Thickness 0.250 mm
ISO 527
 120 MPa
@Thickness 0.125 mm
ISO 527-3
 130 MPa
@Thickness 0.0500 mm
ISO 527-3
 140 MPa
@Thickness 0.0250 mm
ISO 527-3
 65.0 MPa
@Thickness 0.0500 mm,
Temperature 200 °C
ISO 527-3
Film Tensile Strength at Break, TD 110 MPa
@Thickness 0.250 mm
ISO 527-3
 120 MPa
@Thickness 0.0500 mm
ISO 527-3
 120 MPa
@Thickness 0.0250 mm
ISO 527-3
 120 MPa
@Thickness 0.125 mm
ISO 527-3
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cm
@Thickness 0.0500 mm
100 V; ASTM D257
Dielectric Constant 3.5
@Frequency 1e+7 Hz,
Temperature 23.0 °C
0.05 mm; ASTM D150
Dielectric Strength 70.0 kV/in
@Thickness 0.250 mm,
Temperature 23.0 °C
6.25 mm (1/4 inch) electrode; ASTM D149
 120 kV/in
@Thickness 0.125 mm,
Temperature 23.0 °C
6.25 mm (1/4 inch) electrode; ASTM D149
 190 kV/in
@Thickness 0.0500 mm,
Temperature 23.0 °C
6.25 mm (1/4 inch) electrode; ASTM D149
 270 kV/in
@Thickness 0.0250 mm,
Temperature 23.0 °C
6.25 mm (1/4 inch) electrode; ASTM D149
Dielectric Breakdown 6750 V
@Thickness 0.0250 mm,
Temperature 23.0 °C
ASTM D149
 9500 V
@Thickness 0.0500 mm,
Temperature 23.0 °C
ASTM D149
 15000 V
@Thickness 0.125 mm,
Temperature 23.0 °C
ASTM D149
 17500 V
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D149
Dissipation Factor 0.0020
@Frequency 1e+7 Hz,
Temperature 23.0 °C
0.05 mm; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 47.0 µm/m-°C
@Thickness 0.0500 mm
Below Tg; ASTM D696
Shrinkage, MD <= 0.50 %
@Thickness 0.0500 mm,
Temperature 200 °C
TM-VX-84
Shrinkage, TD <= 0.50 %
@Thickness 1.27 mm,
Temperature 200 °C
TM-VX-84
 
Compliance PropertiesOriginal ValueComments
3A-Dairy Yes
FDA YesFDA 21 CFR 177.2415 food compliance
 
Descriptive Properties
Puncture Resistance26 kJ/m20.05 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVICTA48g / 305342

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.