MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ohara S-TIM27 Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: ECO optical glass that does not contain any lead or arsenic.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.76 g/cc2.76 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 1.01.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 560
@Load 0.0999 kg
560
@Load 0.220 lb
Modulus of Elasticity 79.3 GPa11500 ksi
Modulus of Rigidity 32.1 GPa4660 ksi
Poissons Ratio 0.2360.236
Abrasion 141141Aa
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.00 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.44 µin/in-°F
@Temperature -22.0 - 158 °F
 9.90 µm/m-°C
@Temperature 100 - 300 °C
5.50 µin/in-°F
@Temperature 212 - 572 °F
Thermal Conductivity 1.035 W/m-K
@Temperature 35.0 °C
7.183 BTU-in/hr-ft²-°F
@Temperature 95.0 °F
Transformation Temperature, Tg 594 °C1100 °Fper thermal expansion curve
Softening Point 696 °C1280 °F107.65 poise; JIS-R3104 and ASTM-C338
Annealing Point 572 °C1060 °F1013 poise; ASTM-C336
Strain Point 543 °C1010 °F1014.5 poise; JIS-R3103 and ASTM-C336
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.60036
@Wavelength 2325.42 nm
1.60036
@Wavelength 2325.42 nm
 1.60608
@Wavelength 1970.09 nm
1.60608
@Wavelength 1970.09 nm
 1.61249
@Wavelength 1529.58 nm
1.61249
@Wavelength 1529.58 nm
 1.61878
@Wavelength 1128.64 nm
1.61878
@Wavelength 1128.64 nm
 1.62108
@Wavelength 1013.98 nm
1.62108
@Wavelength 1013.98 nm
nt (Hg t line)
 1.62537
@Wavelength 852.11 nm
1.62537
@Wavelength 852.11 nm
ns (Cs s line)
 1.62846
@Wavelength 768.19 nm
1.62846
@Wavelength 768.19 nm
nA' (K A' line)
 1.63138
@Wavelength 706.52 nm
1.63138
@Wavelength 706.52 nm
nr (He r line)
 1.63438
@Wavelength 656.27 nm
1.63438
@Wavelength 656.27 nm
nC (H C line)
 1.63522
@Wavelength 643.85 nm
1.63522
@Wavelength 643.85 nm
nC' (Cd C' line)
 1.63602
@Wavelength 632.8 nm
1.63602
@Wavelength 632.8 nm
nHe-Ne
 1.63964
@Wavelength 589.29 nm
1.63964
@Wavelength 589.29 nm
nD (Na D line)
 1.63980
@Wavelength 587.56 nm
1.63980
@Wavelength 587.56 nm
nd (He D line)
 1.64419
@Wavelength 546.07 nm
1.64419
@Wavelength 546.07 nm
ne (Hg e line)
 1.65294
@Wavelength 486.13 nm
1.65294
@Wavelength 486.13 nm
nf (H F line)
 1.65406
@Wavelength 479.99 nm
1.65406
@Wavelength 479.99 nm
nF' (Cd F' line)
 1.66244
@Wavelength 441.57 nm
1.66244
@Wavelength 441.57 nm
nHe-Cd
 1.66393
@Wavelength 435.835 nm
1.66393
@Wavelength 435.835 nm
ng (Hg g line)
 1.67361
@Wavelength 404.656 nm
1.67361
@Wavelength 404.656 nm
nh (Hg h line)
Abbe Number 34.234.2ν e
 34.4634.46ν d
Optical Dispersion 0.0054240.005424nd-nC; Partial Dispersion
 0.0059160.005916nC-nA'; Partial Dispersion
 0.0089650.008965ne-nC'; Partial Dispersion
 0.009680.00968nh-ng; Partial Dispersion
 0.0098140.009814ne-nC; Partial Dispersion
 0.009870.00987nF'-ne; Partial Dispersion
 0.0109940.010994ng-nF; Partial Dispersion
 0.0132920.013292nC-nt; Partial Dispersion
 0.0141410.014141nC'-nt; Partial Dispersion
 0.0185640.018564nF-nC
 0.0188350.018835nF'-nC'
 0.0241340.024134ng-nd; Partial Dispersion
Transmission, Visible  73 %
@Wavelength 380 nm
73 %
@Wavelength 380 nm
 87 %
@Wavelength 390 nm
87 %
@Wavelength 390 nm
 93.5 %
@Wavelength 400 nm
93.5 %
@Wavelength 400 nm
 97.3 %
@Wavelength 420 nm
97.3 %
@Wavelength 420 nm
 98.3 %
@Wavelength 440 nm
98.3 %
@Wavelength 440 nm
 98.7 %
@Wavelength 460 nm
98.7 %
@Wavelength 460 nm
 99 %
@Wavelength 480 nm
99 %
@Wavelength 480 nm
 99.2 %
@Wavelength 500 nm
99.2 %
@Wavelength 500 nm
 99.6 %
@Wavelength 650 nm
99.6 %
@Wavelength 650 nm
 99.7 %
@Wavelength 550 nm
99.7 %
@Wavelength 550 nm
 99.7 %
@Wavelength 600 nm
99.7 %
@Wavelength 600 nm
 99.7 %
@Wavelength 700 nm
99.7 %
@Wavelength 700 nm
IR Transmittance  91.9 %
@Wavelength 2400 nm
91.9 %
@Wavelength 2400 nm
 93.6 %
@Wavelength 2200 nm
93.6 %
@Wavelength 2200 nm
 98.4 %
@Wavelength 1800 nm
98.4 %
@Wavelength 1800 nm
 99.4 %
@Wavelength 1600 nm
99.4 %
@Wavelength 1600 nm
 99.5 %
@Wavelength 1400 nm
99.5 %
@Wavelength 1400 nm
 99.8 %
@Wavelength 900 nm
99.8 %
@Wavelength 900 nm
 99.8 %
@Wavelength 1000 nm
99.8 %
@Wavelength 1000 nm
 99.8 %
@Wavelength 1200 nm
99.8 %
@Wavelength 1200 nm
 99.9 %
@Wavelength 800 nm
99.9 %
@Wavelength 800 nm
UV Transmittance  5.0 %
@Wavelength 360 nm
5.0 %
@Wavelength 360 nm
 41 %
@Wavelength 370 nm
41 %
@Wavelength 370 nm
 
Descriptive Properties
Acid Resistance, Powder Method, RAP)1
CCI0.00 B
 1.37 G
 1.37 R
coloring, λ 5360
coloring, λ 80390
Coloring, Internal Transmission λ 0.05360
Coloring, Internal Transmission λ 0.80385
Knoop Hardness Class6
Melt Frequency1
Ohara Code d640345
Ohara Code e644342
Ohara StatusPreferred
Phosphate Resistance, PR1
Photoelastic Constant (ß)2.83
Relative Price3.5S-BSL7 = 1
Water Resistance, RW(P)1
Weathering Resistance (Surface Method) W(S)max2
Yield Point, At (°C)629per thermal expansion curve

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CZOHARA963 / 192228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.