MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Label-Lyte™ 612LLG102 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A clear, two-side treated, polypropylene film that is used in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. 612LLG102 is formulated with a proprietary non-migratory slip system. The print surface is treated and can be printed with water-based or solvent-based flexo and gravure inks, and is the intended print and laminating surface. The opposite surface is treated to promote hot melt adhesion.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding clarity and gloss
  • Excellent ink adhesion with solvent-based ink systems
  • Excellent bond strength and most laminating adhesives
  • Contains non-migratory slip system for outstanding performance on roll-fed labeling machines
  • Good hot melt adhesion
Applications:
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
Uses:
  • Reel-Fed Labels
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.500 milExxonMobil Method
Coating Weight 7.10 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 160 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 45 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Coefficient of Friction 0.32Machinable; ExxonMobil Method
Film Tensile Strength at Break, MD 20000 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 38000 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 6.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 6.0 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 1.4 %ExxonMobil Method
Gloss 93 %45°, Machinable Surface; ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.80 receding cos thetaMachinable Surface
 0.85 receding cos thetaHigh Energy Surface
Yield61200 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX99558 / 175794

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.