MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ethydco Advancene™ EM-5204-UVH High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: A high density polyethylene resin is produced via advanced gas phase PE process and is intended for use in injection molding applications such as caps & closures, pails, industrial parts and other shipping containers. This resin has been designed to provide an excellent processability for molders and to meet the rigorous performance characteristics of applications requiring stability, environmental stress crack resistance and impact strength This resin is also suitable for cast film extrusion processing. Main characteristics: for injection molded pails, industrial parts and other shipping containers . For cast film extrusion. Hexene high density resin. Excellent impact strength, stress crack resistance and processability. Very narrow molecular weight distribution.

Mechanical property data for samples molded and tested in accordance with ASTM D4976.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D792
ESCR 100% Igepal® 22 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Index of Compound 4.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240, ISO/IEC 17025:1999
Tensile Strength at Break 31.0 MPaASTM D638, ISO 527
Tensile Strength, Yield 26.9 MPaASTM D638, ISO 527
Elongation at Break 1200 %ASTM D638, ISO 527
Elongation at Yield 9.0 %ASTM D638, ISO 527
2% Secant Modulus 1100 MPaASTM D790B, ISO 178,
Tensile Impact Strength 84.1 kJ/m²Type S; ASTM D1822, ISO 8256
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CASTM D3418, ISO 3146
Crystallization Temperature 119 °CASTM D3418, ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °CUnannealed; ASTM D648, ISO 75
Vicat Softening Point 129 °CASTM D1525, ISO 306
Brittleness Temperature <= 76.0 °CASTM D746, ISO 974( E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethydco Advancene™ EM-6308-UV High Density Polyethylene Resin
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
RTP Company RTP 700 UV High Density Polyethylene (HDPE), UV Stabilized
Ineos T50-500-196 Polyethylene Copolymer

PETHYD919 / 200065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.