Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation plates in moulds, dies, casting tools, presses and similar where the requirements for compression strength and temperature resistance are rigorous. Information provided by Elektro-Isola |
IEC/EN 60893-3-1 PI GC 301, BS 3953 PI-1 |