MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Tungsten 75/Rhenium 25 Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: When used with Tungsten the alloy is an important high temperature thermocouple wire. The alloy can also be used as a filament.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 19.7 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1310 - 2100 MPa
Elongation at Break <= 20 %
Tensile Modulus 370 - 430 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000290 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.48 µm/m-°C
@Temperature 0.000 - 500 °C
Melting Point 3100 °C
 
Component Elements PropertiesOriginal ValueComments
Rhenium, Re 25 %
Tungsten, W 75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
W-25 Re Tungsten Rhenium Alloy, Deformed
W-25 Re Tungsten Rhenium Alloy, Annealed
Goodfellow TZM Molybdenum High Temperature Alloy
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
HWM-25 Molybdenum Alloy

NGOODF246 / 16302

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.