MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
17-7 PH Stainless Steel, TH1050, plate, sheet, and strip
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Processing: TH1050 - heated to austenitic range, 1040°C (1900°F), and water quenched. Reheated to 760°C (1400°F) to precipitate carbides. Carbides cause the austenite transform to martensite after cooling below 15°C (60°F). Tempered at 565°C (1050°)

Applications: high strength high temperature applications, chemical processing equipment, heat exchangers, power boilers, superheater tubes

Corrosion Resistance: 17-7 PH is suitable for use in fresh water, industrial and marine atmospheres, and mild chemical and oxidizing environments. 17-7 PH should not be used in salt water or reducing environments.

Key Words: UNS S17700, double treatment alloy, TH1050, plate, sheet, and strip, 17-7PH, 17-7 PH, 17/7PH, 17/7 PH, Precipitation Hardening
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 38
Tensile Strength, Ultimate 1240 MPaStrength varies with thickness.
Tensile Strength, Yield 1030 MPaStrength varies with thickness.
Elongation at Break 3.0 - 7.0 %
Modulus of Elasticity 204 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000830 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 0.000 - 100 °C
 11.6 µm/m-°C
@Temperature 0.000 - 315 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.4 W/m-K
@Temperature 100 °C
 21.8 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1450 °C
Solidus 1400 °C
Liquidus 1450 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.75 - 1.5 %
Carbon, C <= 0.090 %
Chromium, Cr 16 - 18 %
Iron, Fe 70.6 - 76.8 %as balance
Manganese, Mn <= 1.0 %
Nickel, Ni 6.5 - 7.75 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
17-7 PH Stainless Steel, CH900, plate, sheet, and strip
17-7 PH Stainless Steel, RH950, plate, sheet, and strip
17-7 PH Stainless Steel, RH950, bar and forgings
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
17-7 PH Stainless Steel, TH1050, bar and forgings

MQM177F / 13561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.