MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asia Technology Pioneers CAP 501 PP Nanocomposite
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.

    Advantages:
  • Good paint ability
  • Good dimensional (Heat) stability
  • Outstanding surface appearance
  • UV resistance
  • Hi melt flow
  • Hi Scratch resistance
    Certification:
  • ISO 9001:2008
  • Iranian Nano Technology Initiative Council Certification
  • Certification from automakers
    Application:
  • Automotive Bumpers

Information provided by Asia Technology Pioneers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
Melt Flow 20.9 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 220 kg(f)/cm²ASTM D638M
Flexural Strength 3692 psiASTM D790
Flexural Modulus 13000 kg(f)/cm²ASTM D790
Izod Impact, Notched 49.0 kg-cm/cmASTM D256
 
Descriptive Properties
FormPellets - Gray color
Processing MethodInjection Molding
Reinforcement AdditivesNano Particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shinil Chemical SHINNANO PP Polymer Nanocomposite IP
Noble Polymers Forte™ 4CPP093 Nanocomposite
Noble Polymers Forte™ 35CP091 Nanocomposite
Noble Polymers Forte™ 18CPP091 Nanocomposite
Noble Polymers Forte™ 12HPP093 Nanocomposite

PTATP03 / 135221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.