MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ TC-501 Thermally Conductive Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: LORD CoolTherm™ TC-501 grease is a solvent-free silicone thermal interface material (TIM) designed to replace greases used as TIMs between the heat spreader and the heat sink (commonly known as TIM2). Unlike commercially available greases that eventually pump out, CoolTherm TC-501 grease was developed using proprietary technology that eliminates pump-out. CoolTherm TC-501 grease provides high thermal conductivity and low thermal resistance for applications in which superior heat dissipation is required. CoolTherm TC-501 grease can be used in a variety of packages that cannot go through a cure profile normally required by non-grease TIMs or in applications where greases were previously restricted due to the possibility of pump-out.

Features: eliminates pump-out; provides excellent resistance to moisture and temperature cycling. provides thermal conductivity for applications where superior heat dissipation is required. achieves thin bondlines of 25-50 microns (1-2 mils), minimizing the thermal pathway and maximizing heat flow. easily removed with isopropyl alcohol or acetone, eliminating the use of toxic solvents. easily dispersed; provides a working life of 24 hours at 25°C.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.12 g/cc
Viscosity 128400 cP
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 3.60 W/m-K
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature -30.0 °C
from date of manufacture in original, unopened syringe
 
Descriptive Properties
AppearanceGrey Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9319 / 232675

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.