MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NAECO® ELKONIUM® 18 silver, copper, cadmium alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability in AC circuits. They have low transfer characteristics in some DC applications. The alloying increases the strength and hardness, but substantially reduces the thermal and electrical conductivity and thus limits their current handling capability. The silver-cadmium alloy contacts are ductile materials and can be supplied in shapes and sizes similar to fine silver.

ELKONIUM® 18 alloy, in the spring temper condition, has a proportional limit of 33,000 psi, a modulus of elasticity of 10 X 106 psi, good corrosion resistance and is frequently used as a current carrying spring contact.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.1 g/cc0.365 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 15T 7272annealed
 8585cold worked
Tensile Strength, Ultimate 276 MPa40000 psiannealed
 517 MPa75000 psicold worked
Elongation at Break 3.0 %3.0 %cold worked
 43 %43 %annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cm43 % IACS
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 5.5 %5.5 %
Copper, Cu 7.5 %7.5 %
Nickel, Ni 0.20 %0.20 %
Silver, Ag 86.8 %86.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® ELKONIUM® 23 silver, copper alloy
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy
NAECO® ELKONIUM® 22 silver, copper alloy
NAECO® ELKONIUM® 43 palladium based alloy
CMW® ELKONIUM 1 silver, copper, nickel alloy

NCMV888 / 192373

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.