RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stationery, lamination films, and textile packaging film. Additives: RD734CF contains antiblock and slip agents.Information provided by Borealis AG |