MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Dexflex 711 PCR YZ9A BLACK Thermoplastic Polyolefin
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications.

Dexflex 711 PCR YZ9A BLACK is a thermoplastic olefin elastomeric (TPO) compounded with postindustrial/ post-consumer recycled materials. It is typically used for use in applications that are black but not color-matched, and that require very good processing characteristics. Applications: Exterior Automotive Applications, Underhood.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 16.0 MPa50mm/min, 150 x10 x4 mm specimen; ISO 527-1,-2
Flexural Modulus 1000 MPa2mm/min, 80 x10 x4mm specimen; ISO 178
Impact Test 17.0 J
@Temperature 23.0 °C
Multi-axial Impact Strength
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Engineered Polymer Solutions ABS PCR 400, Recycled
LyondellBasell Dexflex 711 BLK Thermoplastic Polyolefin
LyondellBasell Dexflex 711-300 BLK Thermoplastic Polyolefin
LyondellBasell Hifax Hostacom EYC 2135Y BLACK Polypropylene , Talc Filled
LyondellBasell Hifax Hostacom TRC 103P D72926 Polypropylene , Talc Filled

PEQT7105 / 218742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.