MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reliance Industries Repol B030MG Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: REPOL Polypropylene B030MG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol B030MG is recommended for use in injection molding processes. It is an ideal material for use in crates, furniture, textile and automobile components where medium impact strength is required.

Features:

  • Consistent processability
  • Good stiffness-impact balance
  • Good surface gloss
  • Information provided by Reliance Industries

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Melt Flow 3.0 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 26.5 MPa50mm/min; ASTM D638
    Elongation at Yield 10 %50mm/min; ASTM D638
    Flexural Modulus, 1% Secant 1.00 GPaASTM D790A
    Izod Impact, Notched 110 J/m
    @Temperature 23.0 °C
    ASTM D256
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Reliance Industries Relene M60075 Polyethylene
    Reliance Industries Relene S42005 Polyethylene
    Reliance Industries Relene E52009 Polyethylene
    Reliance Industries Relene E41003 Polyethylene
    Reliance Industries Relene D16501 Polyethylene

    PREL054 / 65394

    Visit Zeus Inc. for PEEK Tubing

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.