MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AISI Type S43035 Stainless Steel annealed 1.6 mm thickness
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Titanium minimum = 0.20 + 4(C+N)

Key Words: UNS S43035, AISI 439 (XM-8), ASME SA240 (XM-8), ASME SA268 (XM-8), ASME SA479 (XM-8), ASTM A240 (XM-8), ASTM A268 (XM-8), ASTM A479 (XM-8), ASTM A651 (XM-8)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 78 - 86
Tensile Strength, Ultimate 483 MPa
Tensile Strength, Yield 328 MPa
Elongation at Break 30 %in 50 mm
Modulus of Elasticity 200 GPaTypical for stainless steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 µm/m-°C
@Temperature 20.0 - 100 °C
 11.5 µm/m-°C
@Temperature 20.0 - 500 °C
 12.4 µm/m-°C
@Temperature 20.0 - 800 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 100 °C
Thermal Conductivity 24.2 W/m-K
@Temperature 0.000 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 17 - 19 %
Iron, Fe 79.8 - 82.8 %
Nitrogen, N <= 0.040 %
Titanium, Ti 0.20 - 1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 439 Ferritic Stainless steel
439 Ferritic Stainless Steel (UNS S43900)
Type 439 Ferritic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S43035
Type 441 Ferritic Stainless Steel, UNS S44100 (Composition Spec)
416 Stainless Steel

MQM43TA / 13807

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.