MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Aclo Accutech Polypropylene Homopolymer HP0336G10M20CL Glass/Mineral Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass/Mineral Reinforced

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inMD; ASTM D955
Melt Flow 3.0 g/10 min3.0 g/10 minASTM D1238
Ash 30 %30 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7878ASTM D785
Tensile Strength at Break 42.0 MPa6090 psiASTM D638
Tensile Strength, Yield 44.0 MPa6380 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 3.499 GPa507.5 ksiASTM D638
Flexural Strength 69.98 MPa10150 psiASTM D790
Flexural Modulus 4.200 GPa609.1 ksiASTM D790
Izod Impact, Notched 0.481 J/cm0.900 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 114 °C237 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Amco PRIMATOP PP HOMO 350NA Injection Molding Polypropylene
Amco PRIMATOP PP HOMO 120NA-HF Multi-Purpose Polypropylene
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Borealis Daploy™ WB140HMS Polypropylene

PACLO180 / 22435

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.