MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Lemalloy® PX603Y PPE-PP Alloy
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: PPE-PP Alloy. High flowability. Lemalloy provides well-balanced mechanical, electrical, and thermal properties. In addition, Lemalloy boasts the lowest specific gravity among engineering plastics. Equipped with the above features, Lemalloy meets market requirements for compactness, high performance, and flame retardance. Stable rigidity, impact strength and fatigue resistance through a wide range of temperatures. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Excellent heat stability. Low specific gravity. Excellent moldability and low shrinkage rate for quality precision parts. Excellent processability; good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
@Thickness 3.20 mm
0.010 - 0.012 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.011 - 0.013 cm/cm
@Thickness 3.20 mm
0.011 - 0.013 in/in
@Thickness 0.126 in
Melt Flow 55 g/10 min
@Load 5.00 kg,
Temperature 280 °C
55 g/10 min
@Load 11.0 lb,
Temperature 536 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psiISO-527-1,2
Tensile Modulus 1.90 GPa276 ksiISO 527-1,2
Flexural Strength 59.0 MPa8560 psiISO 178
Flexural Modulus 1.90 GPa276 ksiISO 178
Charpy Impact Unnotched NBNBISO 179-1,2
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1,2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem H 504 XP Bioriented Film Polypropylene
Hyosung Topilene F600 PP
Braskem H 401 Cast Film Extrusion Polypropylene
LyondellBasell Moplen HP528N Polypropylene
Overview of materials for Polypropylene with 20% Glass Fiber Filler

PMITSU9164 / 191837

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.