MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ganpati Exim HA-991 Titanium Dioxide
Categories: Other Engineering Material

Material Notes: It is a rutile type titanium dioxide product manufactured by chloride process. It is an improved product of the HR-990 series with much better color-killing capacity and weather-resistance. It is of multi-purpose. Higher covering power, lower oil absorption, and better stability, It is comparable with the most high quality products in every quality aspect. HR-991 is widely used in paints, inks, plastic goods paper industry, etc

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles >= 0.85 %
@Load 0.100 kg,
Temperature 105 °C
 
Component Elements PropertiesOriginal ValueComments
TiO2 >= 91 %
 
Descriptive Properties
Brightness>97
Dispersibility (Enterprise Standard)>5
Oil Absorption>23
Tint Reducing Power>100compared with the decided standard sample
 >1820compared with standard sample
Value of Aqueous Suspension7.0-8.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI134 / 317418

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.