MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lucite International Elvacite® 2044 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2044 is a high molecular weight n-butyl methacrylate polymer. Elvacite® 2044 is useful in adhesives for smooth plastic films and aluminum, and in silk screen inks. It will plasticize and improve adhesion of harder butyl grades (Elvacite® 2045 and 2046) and nitrocellulose. Elvacite® 2044 can also be used to improve the outdoor durability of vinyl chloride resins in pigmented lacquers.

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Viscosity Measurement 0.47 - 0.560.47 - 0.56Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 142000 g/mol142000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1.01.0Tukon Hardness
Tensile Strength 3.45 MPa500 psi
Elongation at Break 300 %300 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 20.0 °C68.0 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polycasa Acryl® KR 2007/1 Acrylic
Röhm Plexiglas® 99845 Crystal Clear Elastomer Based Film
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade
Röhm PLEXIGLAS® Film HC 0F028 PMMA
Shinil Chemical SHINCON PMMA Electro Conductive Polymer

PLUCIT9461 / 150175

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.