MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® R 47 HW 10 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion lines, as well as on rod and profile extrusion equipment. Grilon R 47 HW 10 was specially developed for the production of small diameter mandrels which are used for the manufacturing of rubber hoses.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccDry; ISO 1183
Water Absorption 10 %Sim. to ISO 62
Moisture Absorption 2.50 %Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPaDry; ISO 527-1/-2
 46.0 MPaConditioned; ISO 527-1/-2
Tensile Strength, Yield 34.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Conditioned; ISO 527-1/-2
 >= 50 %Nominal, Dry; ISO 527-1/-2
Elongation at Yield 16 %Dry; ISO 527-1/-2
Tensile Modulus 430 MPaConditioned; ISO 527-1/-2
 940 MPaDry; ISO 527-1/-2
Izod Impact, Notched (ISO) 7.50 kJ/m²
@Temperature 0.000 °C
Conditioned; ISO 180/1A
 9.60 kJ/m²
@Temperature 0.000 °C
Dry; ISO 180/1A
 NB
@Temperature 0.000 °C
Conditioned; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 216 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 142 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °CISO 75-1/-2
Vicat Softening Point 159 °C50°C/h 50N; ISO 306
 159 °C50°C/h 50N; ISO 306
 210 °CISO 306
 210 °CISO 306
 
Descriptive Properties
AdditivesPlasticizer
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
Product AttributesFlexible
 High viscosity
 Masterbatch
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nylacast PA6C Cast Nylon 6
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
EMS-Grivory Grilon® F 34 NL PA6
EMS-Grivory Grilon® EB 50 H DZ PA6
EMS-Grivory Grilon® BZ 1/2 PA6

PGRH247 / 156956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.