MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® MDQ23165 + BAYTEC® D22-70MF + BAYTEC® XL B (Catalyst SD6-2) 90 A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccBAYTEC® XL B
 1.17 g/cc1.17 g/ccDESMODUR® MDQ23165
 1.17 g/cc1.17 g/ccBAYTEC® D22-70MF
 1.25 g/cc1.25 g/cc
Viscosity 50 cP50 cPBAYTEC® XL B
 650 cP650 cPBAYTEC® D22-70MF
 1000 cP1000 cPDESMODUR® MDQ23165
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN 53505
 87
@Temperature 80.0 °C
87
@Temperature 176 °F
DIN 53505
 93
@Temperature -5.00 °C
93
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 57.0 MPa8270 psiDIN 53504
Tensile Stress at Strain 3.00 MPa
@Strain 10 %
435 psi
@Strain 10 %
DIN 53504
Elongation at Break 600 %600 %DIN 53504
100% Modulus 8.20 MPa
@Strain 100 %
1190 psi
@Strain 100 %
DIN 53504
200% Modulus 11.4 MPa
@Strain 200 %
1650 psi
@Strain 200 %
DIN 53504
300% Modulus 15.6 MPa
@Strain 300 %
2260 psi
@Strain 300 %
DIN 53504
Resilience 4040[%]; DIN 53512
Tear Strength 58.0 kN/m331 pliwith nick; ISO 34-1
 107 kN/m611 pliwithout nick; ISO 34-1
Abrasion 5050[mm3]; ISO 4649
Compression Set 21 %
@Temperature 70.0 °C,
Time 79200 sec
21 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 35.0 °C95.0 °FDESMODUR® MDQ23165
 35.0 °C95.0 °FBAYTEC® XL B
 70.0 °C158 °FBAYTEC® D22-70MF
Mold Temperature 80.0 °C176 °F
Pot Life 3.50 min3.50 min
 
Descriptive Properties
AppearanceliquidDESMODUR® MDQ23165
 solidBAYTEC® D22-70MF
 solidBAYTEC® XL B
Content0.15SD6-2 % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 14.1Parts by weight of BAYTEC® XL B
 16.2-16.6%NCO
 70Parts by weight of BAYTEC® D22-70MF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur 352 + Baytec 352P + Baytec XL B 76A Polyurethane, MDI Ester
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

PCOVEST0453 / 202236

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.