MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Resin Technology Group CT-523LV Cationic UV Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low outgassing polymer system capable of surviving exposure up to 200°C.

Applications:

Disk drive engineering products, non-acrylic UV bonding. No out gassing concerns. Use as conformal coat and/or wire tack. Opto-Electronic, Fillet-tacking and staking.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 3300 cP
@Temperature 25.0 °C
Uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80Cured
Tensile Strength at Break >= 5000 psiCured
Shear Strength 2200 psiCured, lap
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/milCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °CCured
Minimum Service Temperature, Air -50.0 °CCured
Flash Point >= 200 °FUncured
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear
CompositionEpoxy
Moisture ResistanceExcellentCured
ToxicityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay HTM® 60 Epoxy; HTM60-CF2518-283g/m2-T800 6K 5H satin
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive

PRESINT650 / 65534

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.