MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Eastman Advantis™ 153-2 25X adhesion promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Advantis™ 153-2 25X adhesion promoter is a 25% solution of a chlorinated polyolefin in xylene. It has 21-25 wt. % chlorine and has a Gardner color value of 12-15. Advantis 153-2 25X adhesion promoter has excellent heat stability at temperatures greater than those normally encountered under actual use conditions.

Applications

  • Auto omen
  • Automotive
  • Automotive parts & accessories
  • General industrial coatings
  • Graphic arts
  • Protective coatings
  • Truck/bus/rv

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
 1.105 g/cc0.03992 lb/in³Solid CPO
 
Thermal PropertiesMetricEnglishComments
Flash Point 27.0 °C80.6 °FTag Closed Cup
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 12.0 - 15.012.0 - 15.0
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 21.0 - 25.0 %21.0 - 25.0 %
 
Descriptive Properties
Content<0.1 %Isopropylbenzene (Cumene)
Fire Point30°C
Form (%)25in Xylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4005 / 323628

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.