MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite SUMILITERESIN® PR-F-151 FI Flake phenolic resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: SUMILITERESIN® PR-F-151 FI is a phenolic resin in flake shape with good properties for foundry manufacture. It is designed with a high molecule number and a high softening point. It combines with sticking agents in order to get high performance properties such as anti-peel back, high strength, and a high stick point of resin coated sand (RCS). It is preferable add about 15% hexamine/resin as a hardener when applied in RCS.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 105 - 115 °CB&R
 
Processing PropertiesOriginal ValueComments
Gel Time 1.58 - 2.08 min
@Temperature 150 °C
Resin/hexamine = 100/15
 
Descriptive Properties
AppearanceYellow Flake
Flow Distance25-45mm, 125°C; Resin/hexamine = 100/15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUMIT660 / 194465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.