MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Polybutylene Terephthalate, General Purpose, Flow Modified

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Linear Mold Shrinkage 0.016 - 0.022 cm/cm0.016 - 0.022 in/inASTM D955
Melt Flow 12 - 25 g/10 min
@Load 2.16 kg,
Temperature 250 °C
12 - 25 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7878ASTM D785
Hardness, Rockwell R 117117ASTM D785
Tensile Strength at Break 48.3 MPa7000 psiASTM D638
Tensile Strength, Yield 48.3 MPa7000 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Elongation at Yield 3.5 %3.5 %ASTM D638
Flexural Strength 79.3 MPa11500 psiASTM D790
Flexural Modulus 2.31 GPa335 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Charpy Impact, Notched 0.525 J/cm²
@Temperature 22.8 °C
2.50 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
Gardner Impact 16.9 J12.5 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength  15.4 kV/mm
@Thickness 3.17 mm
390 kV/in
@Thickness 0.125 in
in air; ASTM D149
 15.4 kV/mm
@Thickness 3.17 mm
390 kV/in
@Thickness 0.125 in
in oil; ASTM D149
 22.8 kV/mm
@Thickness 1.59 mm
580 kV/in
@Thickness 0.0625 in
in air; ASTM D149
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C127 °FASTM D648
Vicat Softening Point 190 °C374 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 249 °C450 - 480 °F
Middle Barrel Temperature 238 - 254 °C460 - 490 °F
Front Barrel Temperature 243 - 260 °C470 - 500 °F
Melt Temperature 232 - 260 °C450 - 500 °F
Mold Temperature 43.3 - 76.7 °C110 - 170 °F
Drying Temperature 116 - 121 °C240 - 250 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00127 cm0.000500 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled
Kolon KOCETAL® WR701 Wear Modified Acetal Resin
DuPont Mobility and Materials Delrin® 327UVE RD402 POM

PPOLYQ260 / 160785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.