MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 287 HEC Nylon 6/6 (PA), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Conductive

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccASTM D 792
Additive Loading 40 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23800 psiASTM D 638
Elongation at Break 1.1 %ASTM D 638
Tensile Modulus 2800 ksiASTM D 638
Flexural Strength 39800 psiASTM D 790
Flexural Modulus 2800 ksiASTM D 790
Izod Impact, Notched 1.60 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 12.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness 78 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 81 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 84 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 87 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 91 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 95 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 465 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 540 - 570 °F
Mold Temperature 150 - 225 °F
Drying Temperature 175 °F
@Time 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 CF 30 TS PA 66 reinforced with 30% carbon fibre, thermal stabilization
RTP Company EMI 660.5 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 0899 X 87096 EG BLACK Acetal (POM)
RTP Company RTP 1399X67317C Polyphenylene Sulfide (PPS), GF, Stainless Steel Fiber, EMI
RTP Company RTP 199X67314C Polypropylene, Chemically Coupled, GF, Stainless Steel Fiber, EMI

PQZWA11174 / 90580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.