T50-1000-181 is a lubricated, narrow molecular weight distribution high density polyethylene copolymer intended for general purpose injection molding and extrusion applications. This resin contains a lubrication package for improved release from the mold. This material meets the Food and Drug Administration requirements of 21 CFR 177.1520.Information provided by INEOS |