MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeoGraf GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
Categories: Carbon; Graphite

Material Notes: GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous purity specifications of the nuclear industry, including the General Electric Nuclear Nonmetallic Material Specification D50YP12 (Rev 2) and is typically 99.8% graphite. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 70.0 lb/ft³Standard
Thickness 250 micronsStandard
 380 micronsStandard
 760 micronsStandard
Ash 0.50 %
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Cl (Chloride) <= 10 ppmLeachable
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 525 °C
Minimum Service Temperature, Air -240 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0015 %
Carbon, C 99.5 %
Copper, Cu <= 0.0010 %
Mercury, Hg <= 0.000050 %
Phosphorus, P 0.050 %
Sulfur, S 0.045 %
 
Descriptive Properties
Total Chlorides (%)<50
Total Fluorides (ppm)<50
Total Halogens (ppm)40
Total Nitrates (ppm)10
Total Nitrites (ppm)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
NeoGraf GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced

CGRAF930 / 107334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.