MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for special polymers (PC, PETG, PCTG, PS, ABS, PC/ABS, PMMA etc) to impart permanent static dissipative property. SHINSTAT is directly molded or extruded (film) to achieve the desired level of antistatic property. The level of surface resistivity by SHINSTAT can be varied in the final products depending upon customer needs.

    Feature and Benefits
  • Permanent electrostatic controllability
  • Transparent and colorable
  • Less humidity dependent
  • No particulates
  • Low ionics, out gassing or blooming
  • Recyclability
  • Used for injection molding, film or sheet extrusion
  • Cost effective

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 400 kg(f)/cm²
Flexural Strength 49.05 MPa
Flexural Modulus 17000 kg(f)/cm²
Izod Impact, Notched 5.00 kg-cm/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+9 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 82 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman DuraStar DS2000 Polymer, Natural
Eastman Eastar DN004 PCTG Copolyester
Eastman DuraStar DS1900HF Polymer, Natural
Eastman DuraStar DS1110UVI Polymer, Natural
Eastman DuraStar DS1000 Polymer, Natural

PSHINL48 / 104050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.