MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos XPS PRIME S 30 Extruded polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Synthos XPS PRIME S is characterized by increased thermal insulation, protecting the internal temperature of buildings against the influence of external temperature variability. Constant mechanical strength, durability and resistance to biological agents and chemicals ensure that these boards fulfill their role for many years of use of the building.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.290 - 0.360 g/cc0.0105 - 0.0130 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.200 MPa>= 29.0 psiS 30- I, L, N; perpendicular to faces; EN 1607
 >= 0.400 MPa>= 58.0 psiS 30- IR; perpendicular to faces; EN 1607
Modulus of Elasticity 0.00550 GPa0.798 ksiat 50% of the peak stress; EN 826
 0.0140 GPa2.03 ksiin compression; EN 826
Flexural Strength >= 0.300 MPa>= 43.5 psidN = 60 mm; EN 12089
 >= 0.300 MPa>= 43.5 psidN = 80 mm; EN 12089
 >= 0.400 MPa>= 58.0 psidN = 50 mm; EN 12089
 >= 0.500 MPa>= 72.5 psidN = 40 mm; EN 12089
Compressive Strength >= 0.100 MPa>= 14.5 psi2% deformation; EN 826
 >= 0.110 MPa>= 16.0 psiCompressive creep; EN 1606 + AC
 >= 0.200 MPa>= 29.0 psi5% deformation; EN 826
 >= 0.300 MPa>= 43.5 psi10% relative deformation; EN 826
 >= 0.350 MPa>= 50.8 psiAverage achieved, at 10% deformation; EN 826
Poissons Ratio 0.390.39PN-EN 12090, PN-EN 826
Shear Strength >= 0.0350 MPa>= 5.08 psidN = 160 mm; EN 12090
 >= 0.0400 MPa>= 5.80 psidN = 150 mm; EN 12090
 >= 0.0450 MPa>= 6.53 psidN = 140 mm; EN 12090
 >= 0.0550 MPa>= 7.98 psidN = 120 mm; EN 12090
 >= 0.0750 MPa>= 10.9 psidN = 100 mm; EN 12090
 >= 0.100 MPa>= 14.5 psidN = 80 mm; EN 12090
 >= 0.140 MPa>= 20.3 psidN = 60 mm; EN 12090
 >= 0.190 MPa>= 27.6 psidN = 50 mm; EN 12090
 >= 0.270 MPa>= 39.2 psidN = 40 mm; EN 12090
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C<= 27.8 µin/in-°Fvia thickness; EN 14581
CTE, linear, Parallel to Flow <= 80.0 µm/m-°C<= 44.4 µin/in-°FEN 14581
CTE, linear, Transverse to Flow <= 60.0 µm/m-°C<= 33.3 µin/in-°FEN 14581
Thermal Conductivity  0.0250 W/m-K
@Temperature -60.0 °C
0.174 BTU-in/hr-ft²-°F
@Temperature -76.0 °F
dN = 40-60 mm; EN 14307
 0.0270 W/m-K
@Temperature -60.0 °C
0.187 BTU-in/hr-ft²-°F
@Temperature -76.0 °F
dN = 80-160 mm; EN 14307
 0.0270 W/m-K
@Temperature -40.0 °C
0.187 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
dN = 40-60 mm; EN 14307
 0.0280 W/m-K
@Temperature -40.0 °C
0.194 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
dN = 80-100 mm; EN 14307
 0.0290 W/m-K
@Temperature -40.0 °C
0.201 BTU-in/hr-ft²-°F
@Temperature -40.0 °F
dN = 120-160 mm; EN 14307
 0.0290 W/m-K
@Temperature -20.0 °C
0.201 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
dN = 40-60 mm; EN 14307
 0.0300 W/m-K
@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
dN = 80-100 mm; EN 14307
 0.0310 W/m-K
@Temperature -20.0 °C
0.215 BTU-in/hr-ft²-°F
@Temperature -4.00 °F
dN = 120-160 mm; EN 14307
 0.0310 W/m-K
@Temperature 0.000 °C
0.215 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
dN = 40-60 mm; EN 14307
 0.0320 W/m-K
@Temperature 0.000 °C
0.222 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
dN = 80-100 mm; EN 14307
 0.0320 W/m-K
@Temperature 10.0 °C
0.222 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
dN = 40-60 mm; EN 14307
 0.0340 W/m-K
@Temperature 0.000 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
dN = 120-160 mm; EN 14307
 0.0340 W/m-K
@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 40-80 mm; EN 14307
 0.0340 W/m-K
@Temperature 10.0 °C
0.236 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
dN = 80-120 mm; EN 14307
 0.0350 W/m-K
@Temperature 10.0 °C
0.243 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
dN = 140-160 mm; EN 14307
 0.0360 W/m-K
@Temperature 20.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 100 mm; EN 14307
 0.0360 W/m-K
@Temperature 40.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 40-80 mm; EN 14307
 0.0370 W/m-K
@Temperature 20.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
dN = 120-160 mm; EN 14307
 0.0390 W/m-K
@Temperature 60.0 °C
0.271 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 40-80 mm; EN 14307
 0.0390 W/m-K
@Temperature 40.0 °C
0.271 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 100 mm; EN 14307
 0.0400 W/m-K
@Temperature 70.0 °C
0.278 BTU-in/hr-ft²-°F
@Temperature 158 °F
dN = 40-80 mm; EN 14307
 0.0410 W/m-K
@Temperature 40.0 °C
0.285 BTU-in/hr-ft²-°F
@Temperature 104 °F
dN = 120-160 mm; EN 14307
 0.0420 W/m-K
@Temperature 60.0 °C
0.291 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 100 mm; EN 14307
 0.0450 W/m-K
@Temperature 70.0 °C
0.312 BTU-in/hr-ft²-°F
@Temperature 158 °F
dN = 100 mm; EN 14307
 0.0460 W/m-K
@Temperature 60.0 °C
0.319 BTU-in/hr-ft²-°F
@Temperature 140 °F
dN = 120-160 mm; EN 14307
 0.0490 W/m-K
@Temperature 70.0 °C
0.340 BTU-in/hr-ft²-°F
@Temperature 158 °F
dN = 120-160 mm; EN 14307
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flash Point >= 400 °C>= 752 °FCSN 640149
 
Descriptive Properties
Content<27 mg/kgwater soluble chlorides, EN 13468
 <27 mg/kgwater soluble silicates, EN 13468
 <5 mg/kgwater soluble fluorides, EN 13468
 <5 mg/kgwater soluble sodium ions, EN 13468
Dynamic stiffness100 MN/m3dN = 140 mm; EN 29052-1
 130 MN/m3dN = 120 mm; EN 29052-1
 150 MN/m3dN = 100 mm; EN 29052-1
 190 MN/m3dN = 80 mm; EN 29052-1
 250 MN/m3dN = 60 mm; EN 29052-1
 280 MN/m3dN = 50 mm; EN 29052-1
 38 MN/m3dN = 40 mm; EN 29052-1
 80 MN/m3dN = 160 mm; EN 29052-1
 90 MN/m3dN = 150 mm; EN 29052-1
Point load level>2000 NEN 12430, for 5 mm deformation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNTHOS086 / 320367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.