MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling LAMINEX® 2040 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Application: slippers, gear-rods, bushes

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: PF-7737
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO R 1183
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 170 MPaHc 30; ISO 2039; partially
Tensile Strength, Yield 50.0 MPaISO-DIS 527
Tensile Modulus 7000 MPaDIN 53457
Flexural Strength 80.0 - 100 MPaDIN 54352
Compressive Strength 170 MPaISO 604
Izod Impact, Notched (ISO) 1.50 J/cm²DIN 53453
Izod Impact Resistance 1.80 J/cm²swinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.020With lubrication
Coefficient of Friction, Dynamic 0.020no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+8 ohmDIN 53482
Dielectric Constant 5.0DIN 53483
Dielectric Loss Index 0.30DIN 53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 - 100 °C
DIN 53752
Thermal Conductivity 0.290 W/m-KDIN 52612
Maximum Service Temperature, Air 120 °CContinuous
 150 °CIntermittent
 
Descriptive Properties
Creepage/leakage ResistanceKA1DIN 53480
Moisture Absorption at Equilibrium100 mgDIN 53472

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cookson Group Plaskon® 440 Mineral Filled Novolac Epoxy Molding Compound
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC)

PSCHW036 / 90233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.