MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Lithium Fluoride (LiF)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Solubility 0.27 ppm
a Lattice Constant 4.026 Å
c Lattice Constant 4.026 Å
Molecular Weight 25.94 g/mol
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 980MPa
Hardness, Mohs 4.0
Modulus of Elasticity 88.4 GPain <100> direction
 142.2 GPain <111> direction
Poissons Ratio 0.27
Shear Modulus 40.9 GPain <100> direction
 62.9 GPain <111> direction
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.1 - 34.8 µm/m-°C
@Temperature -60.0 - 60.0 °C
Specific Heat Capacity 1.562 J/g-°C
Thermal Conductivity 14.2 W/m-K
@Temperature 38.0 °C
Melting Point 870 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.101
@Wavelength 10000 nm
 1.262
@Wavelength 7000 nm
 1.3871
@Wavelength 1000 nm
 1.3931
@Wavelength 546.1 nm
at ne
 1.439
@Wavelength 200 nm
IR Transmittance 14 %
@Wavelength 7000 nm
Internal Transmittance
 97 %
@Wavelength 1000 nm
Internal Transmittance
 97 %
@Wavelength 3000 nm
Internal Transmittance
UV Transmittance 90 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(100)perfect
Constants of Elastic Compliance (Pa^-1)1.132E-11S11
 1.591E-11S44
 -3.06E-12S12
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-1.25E-5 to -1.51E-5at 3.39 microns for ± 60°C
Transmission Range (microns)0.12 - 6.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lithium Chloride, LiCl
Lithium Fluoride, LiF
Lithium Oxide, Li2O
Lithium Borohydride, LiBH4
Lithium Borate, LiBO2

CMAT047 / 87731

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.