MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 1090/11 Two-Component General Purpose Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
  • Good Chemical Resistance
  • High temperature
  • Mix Ratio by Weight = 100:10.5
Cure Type: Heat Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.850 g/ccPart A, Loctite Stycast 1090
Density 0.800 g/ccMixed
Water Absorption 0.050 %
@Time 86400 sec
Cured
Viscosity 29000 cPMixed
 35 - 60 cP
@Temperature 35.0 °C
Part B, Loctite CAT 11
Brookfield Viscosity 135000 cPPart A, Loctite Stycast 1090; Speed 10 rpm, # 7
Linear Mold Shrinkage 0.0020 cm/cm
Outgassing - Total Mass Loss 0.38 %
Collected Volatile Condensable Material 0.040 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Tensile Strength 4700 psi
Flexural Strength 44.0 MPaASTM D790
Compressive Strength 82.7 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 2.73
@Frequency 1e+6 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.050
@Frequency 0.001 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°CBelow Tg; TMA
Thermal Conductivity 0.190 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 hour
@Temperature 120 °C
Option 3, Post Cure: 2 to 4 hours at the highest expected use temperature
 2.00 - 4.00 hour
@Temperature 100 °C
Option 2, Post Cure: 2 to 4 hours at the highest expected use temperature
 8.00 - 16.0 hour
@Temperature 80.0 °C
Option 1, Post Cure: 2 to 4 hours at the highest expected use temperature
Working Life >= 240 min
@Temperature 25.0 °C
100 g mass
Shelf Life 12.0 MonthPart A, Loctite Stycast 1090
 
Descriptive Properties
AppearanceBlackAlso available in the color white
Mix Ratio, by Weight100 : 10.5Resin : Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Trelleborg Emerson & Cuming Stycast® 1265 Two-Component Easy Mix Ratio Encapsulant
Alclad Aluminum 7075-T6, T651
Isoflon PEHD 1000 High Density Polyethylene
Titanium, Ti

PEMERS40 / 35732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.