MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Exceptional Colorability - Outstanding Adhesion in Both Two-Shot and Insert Molding Processes - Soft, Rubbery Grip - Very Easy to Process

Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 6059-9 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versaflex™ OM 6059-9 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 3 to 6 in/sec 1st Stage - Boost Pressure: 300 to 800 psi 2nd Stage - Hold Pressure: 0% of Boost Hold Time (Thick Part): 0 to 4 sec Hold Time (Thin Part): 0 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Viscosity  16900 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
16900 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 75000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
75000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 585810 sec; ASTM D2240
Tensile Strength at Break 2.45 MPa
@Temperature 23.0 °C
355 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.75 MPa
@Strain 100 %,
Temperature 23.0 °C
254 psi
@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 290 %
@Temperature 23.0 °C
290 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set  14 %
@Temperature 22.0 °C,
Time 79200 sec
14 %
@Temperature 71.6 °F,
Time 22.0 hour
ASTM D395B
 63 %
@Temperature 70.0 °C,
Time 79200 sec
63 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 204 °C360 - 399 °F
Middle Barrel Temperature 243 - 266 °C469 - 511 °F
Front Barrel Temperature 249 - 271 °C480 - 520 °F
Nozzle Temperature 254 - 277 °C489 - 531 °F
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 12.8 - 29.4 °C55.0 - 84.9 °F
Back Pressure 0.000 - 0.552 MPa0.000 - 80.1 psi
Screw Speed 80 - 120 rpm80 - 120 rpm
 
Descriptive Properties
Agency RatingsUL 94 .QMFZ2.E76261
AppearanceBlack
FeaturesGood Adhesion
 Good Colorability
 Good Processability
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Suggested Max Regrind20%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
Avient Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE)
Avient Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
API Megol AM DP2154 SEBS Adhesion Modified Overmolding for PA
Avient Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)

PH0POL1208 / 145777

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.