MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ THERMOCOMP™ D351RC PC (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP* THERMOCOMP* D351RC compound is based on Polycarbonate resin containing Glass Fiber and Flame Retardant. Added features of this material includes high modulus, good flatness, good impact performance, Non-Halogenated Flame Retardant, PCR content up to 35%.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.425 g/cc0.05148 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Time 86400 sec
0.0010 - 0.0030 in/in
@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm
@Time 86400 sec
0.0010 - 0.0030 in/in
@Time 24.0 hour
ASTM D955
Melt Flow 27.3 g/10 min
@Load 2.16 kg,
Temperature 300 °C
27.3 g/10 min
@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 129 MPa18700 psi5 mm/min; ASTM D638
Elongation at Break 2.2 %2.2 %5 mm/min; ASTM D638
Tensile Modulus 9.415 GPa1366 ksi5 mm/min; ASTM D638
Flexural Strength 180 MPa26100 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.39 GPa1220 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.28 J/cm2.40 ft-lb/inASTM D256
Izod Impact, Unnotched 5.37 J/cm10.1 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 68.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 119 °C
@Thickness 3.20 mm
246 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 285 - 305 °C545 - 581 °FInjection Molding
Zone 1 260 - 280 °C500 - 536 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 285 - 310 °C545 - 590 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hourInjection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.100 - 0.300 MPa14.5 - 43.5 psi
Screw Speed 50 - 90 rpm50 - 90 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI13450 / 246917

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.