MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oceanchem Group 1,2,5,6,9,10-Hexabromocyclododecane (HBCD)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C12H18Br6

Cas No.: 3194-55-6

Characteristics: The product is white crystalline powder, melting point greater than 180°C, bromine content greater than or equal to 73%. This product is soluble in alcohols, ketones andesters, such as organic solvents such as methanol, ethanol, amyl acetate, acetone and so on. This product should be stored in a cool, dry, ventilated warehouse, in the store and transportation process should be handled with care to prevent impact damage.

Use: It is used as flammable inhibitor for EPS, polypropylene fibre and styrene resin, it is also used as an adding agent of flammable inhibitor for polyethylene, poly carbonate, unsaturated polester. It can be used in fire-proof treatment of fabric, butadiene styrene rubber, binder, coating and unsaturated polyester.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.50 %
@Temperature 110 °C,
Time 7200 sec
0.50 %
@Temperature 230 °F,
Time 2.00 hour
Molecular Weight 641.7 g/mol641.7 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 - 185 °C352 - 365 °FOrdinary type
 185 - 195 °C365 - 383 °FHigh melting point
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 74.0 - 75.0 %74.0 - 75.0 %
 
Descriptive Properties
CAS Number3194-55-6
Hue APHA<30
Molecular FormulaC12H18Br6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Fluoroborate Hexahydrate, Zn(BF4)2-6H2O
Solvay RHODAFAC® RS-610/A25 Surfactant
LG Chemical R320 EPS, Flame Retardant
LG Chemical R240 EPS, Flame Retardant
LG Chemical R160 EPS, Flame Retardant

POCEAN06 / 104210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.