MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2050712D58 Silver Ink for ITO Substrates
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental and abrasion resistance with good flexibility and adhesion to alternative ITO coated substrates.

This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use to ensure complete homogeneity.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 54.9 - 55.1 %
Viscosity 6000 - 10000 cP
@Shear Rate 50 1/s,
Temperature 25.0 °C
Haake VT550 cone and plate viscometer with the PK1.1°
Thickness 16.0 - 18.0 micronsCured film
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.055 ohmat 25 microns thick
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 min
@Temperature 130 °C
belt dryer
 10.0 min
@Temperature 130 °C
box oven
Shelf Life 3.00 Monthat 20°C maximum
 6.00 Monthat 5°C maximum
 
Descriptive Properties
Coverage cm2/g200230 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VP Disp. ITO LUV2 Conductive lacquer
Indium Corp. Standard ITO Indium Tin Oxide
Indium Corp. Fine ITO Indium Tin Oxide
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window

WGEM016 / 75869

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.