MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL LL4F 808-SB Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL LL4F 808-SB is ethylene 1-butene LLDPE resin designed for the blown film. It has good stiffness and tensile strength. These resin’s strength and drawability make them excellent for many film applications.

Recommended Applications: Industrial packaging, heavy duty sacks, general purpose packaging and bags needing moderate clarity.

Additives: Antiblock – 3500 ppm, Slip – 1250 ppm..

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D1505
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3500 ppm
Slip Level 1250 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1400 psiASTM D882
Film Tensile Strength at Yield, TD 1600 psiASTM D882
Film Elongation at Break, MD 610 %ASTM D882
Film Elongation at Break, TD 870 %ASTM D882
1% Secant Modulus 30500 psiMD; ASTM D882
 33000 psiTD; ASTM D882
Elmendorf Tear Strength MD 100 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test <= 110 gASTM D1709A
Film Tensile Strength at Break, MD 6500 psiASTM D882
Film Tensile Strength at Break, TD 4800 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 123 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D1003
Gloss 57 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO123 / 283720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.