MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Socomore Chemglaze® A080 Polyurethane Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Chemglaze® A-line coatings are moisture-curing, aliphatic polyurethane coatings designed for product finishing applications on many metal and rigid or semirigid plastic substrates. Chemglaze A-Line coatings are ASTM D-16 Type II oil-free products, and are available in clear, black and white.

Features:

  • Versatile: perform well in many metal and plastic product finishing applications. Durable high gloss finish can be adjusted to semigloss or lusterless by adding Chemglaze A170 flatting concentrate.
  • Durable: provide excellent resistance to impact and abrasion; exhibit low Taber weight loss values.
  • Environmentally Resistant: provide long-term weathering resistance properties.
  • Chemically Resistant: cure to a hard surface that is resistant to many acids, alkalines, detergents, lubricating oils, solvents and chemicals.
  • Color Retention: provide excellent colorfast, high gloss finish.
Use Chemglaze 9951 thinner, xylene, methyl ethyl ketone (MEK) or methyl isobutyl ketone (MIBK) to clean equipment before coating dries. Do not use lacquer thinners, water or solvents containing alcohols.

Information provided by Socomore.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 - 1.02 g/ccAs Supplied; ASTM D1475
Solids Content 58.8 - 63.2 %ASTM D2369 mod.
Volatile Organic Compounds (VOC) Content 407 g/lASTM D3960
Brookfield Viscosity 450 - 925 cPSpindle 2; 30 RPM; ASTM D2196
 
Thermal PropertiesOriginal ValueComments
Flash Point 28.0 °CSeta, Closed Cup; ASTM D3278
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 10.0 - 32.0 °C
in original, unopened container
 
Descriptive Properties
AppearanceClear LiquidAs Supplied

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOCOM991 / 248985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.