MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Bayflex® 110-35 Urethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Bayflex 110-35 system produces a solid urethane elastomer which has a flexural modulus of approximately 33,500 psi* at room temperature.

Properties / Applications: Bayflex 110-35 system produces a solid urethane elastomer which has a flexural modulus of approximately 33,500 psi* at room temperature. This system is used to produce large reaction injection molding (RIM) parts, such as automotive fascias. The system combines rapid demold times, excellent integrity at demold, and outstanding physical properties. Bayflex 110-35 is a formulated RIM system supplied as two liquid components. Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. As with any product, use of the Bayflex 110-35 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D1622
 1.03 g/cc1.03 g/ccPolyol (Component B)
 1.21 g/cc1.21 g/ccIsocyanate (Component A)
Viscosity 700 cP700 cPIsocyanate (Component A)
 1300 cP1300 cPPolyol (Component B)
Linear Mold Shrinkage 0.0056 cm/cm0.0056 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 20.7 MPa3000 psiASTM D638
Elongation at Break 220 %220 %ASTM D638
Tensile Modulus 0.0134 GPa1.94 ksiASTM D412
Flexural Modulus  0.134 GPa
@Temperature 65.0 °C
19.4 ksi
@Temperature 149 °F
ASTM D412
 0.231 GPa
@Temperature 23.0 °C
33.5 ksi
@Temperature 73.4 °F
ASTM D412
 0.469 GPa
@Temperature -30.0 °C
68.0 ksi
@Temperature -22.0 °F
ASTM D412
Izod Impact, Notched 2.67 J/cm5.00 ft-lb/inASTM D624
Tear Strength 61.4 kN/m350 pliDie C
 
Thermal PropertiesMetricEnglishComments
Flash Point 149 °C300 °FPolyol (Component B)
 213 °C415 °FIsocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 66.0 °C151 °F
 
Descriptive Properties
AppearanceLight brown to pale tan liquidPolyol (Component B)
 Light yellow to yellow liquidIsocyanate (Component A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8660E Urethane Elastomer
Covestro Bayflex® 110-50 Urethane Elastomer
Covestro Bayflex® 110-35 IMR Urethane Elastomer
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf

PCOVEST0117 / 201900

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.