MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Shanghai Potomer MBS-600 PVC Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Brief Introduction: PVC Impact Modifier MBS-600 is the tercopolymer of methyl methacrylate(M), butadiene(B), styrene(S) , mainly used in the process of shaping PVC. The main characteristics of PVC Impact Modifier MBS-600 is that it provides PVC products with high impact resistance, good processability and reduced gelation time.

Applications: PVC Impact Modifier MBS-600 is mainly used in opaque planking, tubing, profile shapes, pipe fittings for indoor use, to improve their impact strength.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.250 - 0.500 g/cc0.00903 - 0.0181 lb/inĀ³
Volatiles 1.0 %1.0 %
Particle Mesh Size 20 Mesh20 Mesh0.98
 
Descriptive Properties
Color/AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM197 / 284643

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.