MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos CM3588M Chlorinated Polyethylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chlorinated polyethylene is a heat, weathering and oil resistant elastomer that has used in many wire/cable, hose, automotive and industrial parts for many years.

Characteristics: High molecular weight, slightly lower Mooney viscosity than CM3595NC, superior mechanical performances and easy for formulation

Application: Medium to high viscosity grade for improved extrusion and good mechanical properties at higher filler loadings.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.20 %0.20 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555
Tensile Strength 12.5 MPa1810 psi
Elongation at Break 800 %800 %
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1.00 J/g0.430 BTU/lb
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 35 %35 %
 
Descriptive Properties
AppearanceWhite powder
Content10 piece/100gImpurity particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW227 / 320258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.