MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion ToughMet® 3 AT110 Tube, Copper Nickel Tin Alloy (TX00) 0.595 to 3.9 in (C72900)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: ToughMet® is used for severe service material problems.
  • Exceptional resistance to corrosion and cavitation
  • Outstanding lubricity and durability in demanding applications
  • Highly uniform composition in all product forms
  • Uniform microstructure in a variety of wrought shapes and sizes

ToughMet® 3 in the wrought and spinodally hardened (AT) condition exhibits tensile strength up to 140 ksi and hardness up to HMRC 34 in a Copper-15% Nickel-8% Tin alloy with excellent machinability.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 30.030.0
Tensile Strength >= 862 MPa>= 125000 psi
Tensile Strength, Yield >= 758 MPa
@Strain 0.200 %
>= 110000 psi
@Strain 0.200 %
Elongation at Break >= 10.0 %
@Thickness 50.8 mm
>= 10.0 %
@Thickness 2.00 in
Modulus of Elasticity 145 GPa21000 ksi
Fatigue Strength 276 - 414 MPa
@# of Cycles 1.00e+7
40000 - 60000 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000190 - 0.0000246 ohm-cm0.0000190 - 0.0000246 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C9.10 µin/in-°F
Thermal Conductivity 38.05 W/m-K
@Temperature 100 °C
264.1 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 76.0 - 78.0 %76.0 - 78.0 %
Nickel, Ni 14.5 - 15.5 %14.5 - 15.5 %
Tin, Sn 7.50 - 8.50 %7.50 - 8.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBBC11q / 323401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.