MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
AMG Aluminum 20% Calcium Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Aluminum mechanical and physical properties are enhanced with the use of alloying elements. These alloying elements are commonly referred to as hardeners. Aluminum based master alloys which contain the hardener elements in high concentrations, provide a convenient and economical way to add them to aluminum to achieve desired properties. These master alloys readily go into solution at lower liquid temperatures, thus minimizing dross formation and solubility of hydrogen. Lower furnace temperatures also mean reduced energy consumption and longer furnace life.

Information provided by KB Alloys

Al. Assoc. Registration No: H2000

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 77.32 - 81.32 %
Calcium, Ca 18 - 22 %
Iron, Fe 0.30 %
Other, each 0.030 %
Other, total 0.10 %
Silicon, Si 0.20 %
Vanadium, V 0.050 %
 
Descriptive Properties
FormWaffle Ingot, Slab Ingot, Super Slab

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AMG Aluminum 15% Strontium Aluminum Alloy
AMG Aluminum 12% Strontium Aluminum Alloy
Mitsubishi IupilonĀ® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Mitsubishi IupilonĀ® H-2000 Polycarbonate

NKBAL32 / 17702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.