Notes: 60AIM is an unfilled, lightly modified nylon 6 injection molding grade that is designed for use where improved toughness, coupled with good rigidity is required.Availability: Europe; North America Features: Good Toughness; Medium Rigidity Processing Method: Injection Molding Information provided by Teknor Apex |