MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Honeywell Genetron® AZ-50 Refrigerant
Categories: Fluid

Material Notes: Genetron® AZ-50® refrigerant (an azeotropic mixture of HFC-125 and HFC-143a, assigned R-507 by ASHRAE) was developed by Honeywell to serve as a long-term substitute for the refrigerant R-502. This patented, environmentally safe, non-ozone-depleting substitute possesses similar energy efficiency and capacity characteristics to R-502 and has an intrinsically low toxicity. Genetron AZ-50 has higher energy efficiency than other R-502 alternatives, due in part to superior heat transfer characteristics. Genetron AZ-50 is an excellent refrigerant choice for low- and medium-temperature refrigeration applications. Genetron® 404A is a refrigerant blend made up of HFC-125, HFC-143a, and HFC-134a and assigned the refrigerant number R-404A by ASHRAE. Like Genetron AZ-50, Genetron 404A is a non-ozone-depleting long-term alternative to R-502 that is well suited for low- and medium-temperature refrigeration applications.

Applications: In commercial refrigeration, Genetron AZ-50 and Genetron 404A serve a wide range of applications including supermarket freezer cases, reach-in coolers, display cases, transport refrigeration, and ice machines. These refrigerants may also be used to replace R-502 in a number of specialty applications. Genetron AZ-50 and Genetron 404A are suitable for both new equipment and retrofitting existing R-502 commercial refrigeration systems. Generally, there will be few, if any, equipment changes necessary to optimize the performance of Genetron AZ-50 or Genetron 404A refrigerants in these applications. For retrofitting commercial systems, refer to bulletin G525-100, Genetron Refrigeration Retrofit Guidelines.

Chemical Name: Pentafluoroethane/1,1,1-Trifluoroethane

Molecular Formula : CHF2CF3 (50%) / CH3CF3 (50%)

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.005586 g/cc0.0002018 lb/in³Vapor at boiling point
 0.49080 g/cc0.017730 lb/in³Critical
 1.048 g/cc0.03786 lb/in³Liquid
Volatiles 100 %100 %
Viscosity 14.58 cP14.58 cPVapor
 127.6 cP127.6 cPLiquid
Molecular Weight 98.9 g/mol98.9 g/mol
Vapor Pressure 12.83 bar9620 torr
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 37.05 bar27790 torr
Critical Temperature 70.617 °C159.11 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 197.2 J/g84.72 BTU/lbat boiling point
Specific Heat Capacity 1.55 J/g-°C0.370 BTU/lb-°FLiquid
 0.870 J/g-°C
@Pressure 0.101 MPa
0.208 BTU/lb-°F
@Pressure 14.7 psi
Vapor
Thermal Conductivity 0.0180 W/m-K0.125 BTU-in/hr-ft²-°FVapor
 0.0639 W/m-K0.443 BTU-in/hr-ft²-°FLiquid
Melting Point 80.94 - 82.94 °C
@Pressure 0.101 MPa
177.7 - 181.3 °F
@Pressure 14.7 psi
Boiling Point -46.7 °C
@Pressure 0.101 MPa
-52.1 °F
@Pressure 14.7 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHONWL135 / 179680

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.