MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the black mode.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccSTN EN ISO 1183-1
Linear Mold Shrinkage 0.018 cm/cmSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cmSTN EN ISO 294-4
Melt Flow 5.0 g/10 min
@Load 0.325 kg,
Temperature 275 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPaSTN EN ISO 527-2
Elongation at Break 3.5 %STN EN ISO 527-2
Tensile Modulus 3500 MPaSTN EN ISO 527-2
Flexural Strength 95.0 MPaSTN EN ISO 178
Flexural Modulus 2900 MPaSTN EN ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
STN EN ISO 179
 NB
@Temperature -20.0 °C
STN EN ISO 179
Charpy Impact, Notched 3.50 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 3.50 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CSTN EN ISO 75-2 (A)
Vicat Softening Point 250 °CSTN EN ISO 306
Flammability, UL94 V-2
@Thickness 3.20 mm
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
STN EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 260 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
@Time 14400 sec
Moisture Content 0.25 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized
Nylene® Nylene 137 HS UV BK Nylon 66, Heat Stabilized
Nylene® Nylene 132L Nylon 66, Heat Stabilized
Nylene® Nylene 132 HSL Nylon 66, Heat Stabilized

PPLACO631 / 140902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.